Part 1 - Silver Clay
You Will Need: A kiln, a steel mesh, a firing fork
Place your silver clay piece on a steel mesh and put it in a room temperature kiln. Bring the kiln up to temperature over at least 15 minutes and then fire at 650C /1200F for at least 30 minutes. Other firing times and temperatures are available so make sure you have read the manufacturers instructions for the clay you are using before firing. Once fully fired, remove the pieces from the kiln and leave to cool naturally.